𝔖 Bobbio Scriptorium
✦   LIBER   ✦

NON-DESTRUCTIVE SURFACE ANALYSIS OF ROMAN TERRA SIGILLATA: A POSSIBLE TOOL IN PROVENANCE STUDIES?

✍ Scribed by P. J. BALLIÉ; W. B. STERN


Book ID
115284242
Publisher
John Wiley and Sons
Year
1984
Tongue
English
Weight
350 KB
Volume
26
Category
Article
ISSN
0003-813X