Nanoscale mechanical characterization of PMMA by AFM nanoindentation: a theoretical study on the time-dependent viscoelastic recovery
✍ Scribed by Ding, Y. H.; Deng, X. H.; Jiang, X.; Zhang, P.; Yin, J. R.; Jiang, Y.