Nanoindentation of injection molded PLA and self-reinforced composite PLA after in vitro conditioning for three months

✍ Scribed by Debra D. Wright-Charlesworth; Darinda M. Miller; Ibrahim Miskioglu; Julia A. King


Publisher
John Wiley and Sons
Year
2005
Tongue
English
Weight
306 KB
Volume
74A
Category
Article
ISSN
1549-3296

No coin nor oath required. For personal study only.

✦ Synopsis


Abstract

Poly(lactic acid) (PLA) is used for medical devices such as sutures or orthopedic screws. A standard way to determine the loss of mechanical properties of a degradable polymer would be to soak the polymer in phosphate buffered saline (PBS) and test the desired property as a function of immersion time. This method is not sensitive enough to discern changes in mechanical properties through the cross‐section of the polymer and neglects the degradation that is occurring at the molecular level. This article presents results of a nanoindentation study carried out with PLA. The modulus and hardness of PLA is characterized as a function of processing method, immersion time in PBS, and location of the indent. Measuring local properties with the nanoindenter allowed detection of differences in material properties as a function of all three of these variables. The mechanical properties on the edge were lower than the interior of the sample after in vitro degradation, and changes were seen earlier for nanoindentation than for traditional flexural or tensile tests. The nanoindenter is a valuable tool for quantifying changes in material properties and may have applicability for accelerated tests to screen biomaterials. © 2005 Wiley Periodicals, Inc. J Biomed Mater Res, 2005