Nanoindentation creep of tin and aluminium: A comparative study between constant load and constant strain rate methods

✍ Scribed by Lu Shen; Wun Chet Davy Cheong; Yong Lim Foo; Zhong Chen


Book ID
113809971
Publisher
Elsevier Science
Year
2012
Tongue
English
Weight
777 KB
Volume
532
Category
Article
ISSN
0921-5093

No coin nor oath required. For personal study only.