Nanoindentation and nanoscratch investigations on graphene-based nanocomposites

✍ Scribed by M.M. Shokrieh; M.R. Hosseinkhani; M.R. Naimi-Jamal; H. Tourani


Book ID
119351930
Publisher
Elsevier Science
Year
2013
Tongue
English
Weight
990 KB
Volume
32
Category
Article
ISSN
0142-9418