Nanoindentation analysis for local properties of ultrafine grained copper processed by high pressure torsion

✍ Scribed by Jeong, Hyeok Jae; Yoon, Eun Yoo; Lee, Dong Jun; Kim, Nack Joon; Lee, Sunghak; Kim, Hyoung Seop


Book ID
115439814
Publisher
Springer
Year
2012
Tongue
English
Weight
496 KB
Volume
47
Category
Article
ISSN
0022-2461

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Local thermal property analysis by scann
✍ F.A. Guo; Y.L. JI; N. Trannoy; J. Lu πŸ“‚ Article πŸ“… 2006 πŸ› Elsevier Science 🌐 English βš– 454 KB

Scanning thermal microscopy (SThM) was used to map thermal conductivity images in an ultrafine-grained copper surface layer produced by surface mechanical attrition treatment (SMAT). It is found that the deformed surface layer shows different thermal conductivities that strongly depend on the grain