Multi-objective optimization of Nd:YAG laser cutting of nickel-based superalloy sheet using orthogonal array with principal component analysis

โœ Scribed by Avanish Kumar Dubey; Vinod Yadava


Publisher
Elsevier Science
Year
2008
Tongue
English
Weight
220 KB
Volume
46
Category
Article
ISSN
0143-8166

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Multi-objective optimization of Nd:YAG l
โœ Raghavendra Rao; Vinod Yadava ๐Ÿ“‚ Article ๐Ÿ“… 2009 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 382 KB

This paper presents a hybrid optimization approach for the determination of the optimum laser cutting process parameters which minimize the kerf width, kerf taper, and kerf deviation together during pulsed Nd:YAG laser cutting of a thin sheet of nickel-based superalloy SUPERNI 718 (an equivalent gra