Morphology and mechanical properties of composites based on polyamide 6 and mineral additives
β Scribed by H. Unal
- Publisher
- Elsevier Science
- Year
- 2004
- Weight
- 248 KB
- Volume
- 25
- Category
- Article
- ISSN
- 0261-3069
No coin nor oath required. For personal study only.
β¦ Synopsis
Polyamide 6 composites filled with up to 30 wt% spherical glass beads, and flake-like talc fillers, were prepared by extrusion and injection moulding. One or more than one filler, with weight percentages varying between 10 and 30 wt%, were added to polyamide 6. Uniaxial tensile, impact and three-point bending tests were used to examine the effect of filler addition on the mechanical behaviour of polyamide 6. Tensile strength, elongation at break, modulus of elasticity impact energy and flexural strength and modulus were obtained. The results showed that the tensile strength and modulus of elasticity of polyamide 6 composite linearly increased with the increase in filler weight ratio while the impact strength and maximum elongation linearly decreased with the increase in filler weight ratio. The overall maximum improvement in mechanical properties was recorded with the addition of 10-20 wt% filler ratios.
π SIMILAR VOLUMES
## Abstract In this investigation, the influence of filler type and filler content on the mechanical properties of nylonβ6 is investigated. The mineral fillers were selected on the basis of their shape and size: flakeβlike kaolin and talc, spherical glass beads or fibrous wollastonite. These filler