✦ Synopsis


The silicone-EPDM system has been studied with blend ratios (silicone: EPDM) of 50:50, 40:60 and 30:70. The first set of blends was prepared by roll-mixing of the elastomers and curative whereas in the second set, DCP-cured powder of EPDM, prepared in a Brabender plasticorder, was mixed with silicone rubber and DCP in a roll mill. A comparison of blends show that the second set exhibits inferior properties as compared to the first set. Specimens were also aged at 1 50 and 175 ~ for various periods. The physical properties of the aged specimens show a reversal in trend, i.e. the second set of specimens shows better physical properties on ageing. The strengthening of the silicone phase by use of a different curative (Perkadox 14/40) in the 50:50 blend of the second set shows a beneficial action on ageing. Morphology studies with SEM confirm the two-phase structure for both sets of blends. In both cases phase separation occurs with ageing, but the continuous phase for the second set of blends maintains its continuity for a higher period than the corresponding specimens of the first set.


πŸ“œ SIMILAR VOLUMES


Morphology and permeability of polymer b
✍ Y. Geerts; S. Gillard; G. Geuskens πŸ“‚ Article πŸ“… 1996 πŸ› Elsevier Science 🌐 English βš– 257 KB

EPDM-silicone rubber blends prepared by melt mixing have been compression moulded into sheets and crosslinked by gamma irradiation. The permeability of the blends to methanol vapour has been measured at room temperature. It changes progressively with membrane composition and no threshold can be dete

Surface properties of EPDM, silicone rub
✍ Anil K. Bhowmick; J. Konar; S. Kole; S. Narayanan πŸ“‚ Article πŸ“… 1995 πŸ› John Wiley and Sons 🌐 English βš– 519 KB

Surface energy of EPDM, silicone rubber, and their 50 : 50 (by weight) blend during aging was determined by contact angle measurement using water and formamide as the probe liquids. The surface energy increases initially with aging time. The results are explained on the basis of the polar component

Accelerated hydrothermal weathering of s
✍ S. Kole; S. K. Srivastava; D. K. Tripathy; A. K. Bhowmick πŸ“‚ Article πŸ“… 1994 πŸ› John Wiley and Sons 🌐 English βš– 545 KB

Hydrothermal weathering of the peroxide vulcanized specimens of silicone rubber, EPDM rubber, and their 50 : 50 blend carried out for various durations a t different temperatures reveals that silicone is very susceptible to degradation. For example, the modulus, the strength, and the elongation at b