๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Modulated differential scanning calorimetry in the glass transition region

โœ Scribed by B. Wunderlich; A. Boller; I. Okazaki; S. Kreitmeier


Publisher
Springer Netherlands
Year
1996
Tongue
English
Weight
791 KB
Volume
47
Category
Article
ISSN
0022-5215

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Modulated differential scanning calorime
โœ Iwao Okazaki; Bernhard Wunderlich ๐Ÿ“‚ Article ๐Ÿ“… 1996 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 972 KB

Temperature-modulated differential scanning calorimetry is used to evaluate the kinetics of the glass transition from measurement of the first harmonic of the apparent, reversing heat capacity. The data are taken from quasi-isothermal experiments with negligible instrument lag, extrapolated to zero