Modulated differential scanning calorimetry: 6. Thermal characterization of multicomponent polymers and interfaces
β Scribed by D.J. Hourston; M. Song; A. Hammiche; H.M. Pollock; M. Reading
- Book ID
- 108367118
- Publisher
- Elsevier Science
- Year
- 1997
- Tongue
- English
- Weight
- 539 KB
- Volume
- 38
- Category
- Article
- ISSN
- 0032-3861
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
The purpose of this study was to characterize the thermal properties of microcrystalline cellulose (MCC) and to investigate the inΒ―uence of water on these properties. Differential scanning calorimetry (DSC), modulated temperature differential scanning calorimetry (MTDSC), thermomechanical analysis (
The objective of the present study was to characterize the glassy state of ketoconazole and to calculate its molecular mobility below the glass transition, with a view to further developing the use of modulated temperature differential scanning calorimetry (MTDSC) as a means of studying relaxation b
## Abstract Temperature modulated differential scanning calorimetry (TMDSC) was employed to study the melting and crystallization behavior of various polyethylenes (PEs). Samples of high density PE (HDPE), low density PE (LDPE), linear low density PE (LLDPE), and very low density PE (VLDPE) with di