Microtensile bond strength of composite resin to glass-infiltrated alumina composite conditioned with Er,Cr:YSGG laser
✍ Scribed by Carlos de Paula Eduardo; Marina Stella Bello-Silva; Simone Gonçalves Moretto; Paulo Francisco Cesar; Patricia Moreira de Freitas
- Publisher
- Springer-Verlag
- Year
- 2010
- Tongue
- English
- Weight
- 526 KB
- Volume
- 27
- Category
- Article
- ISSN
- 0268-8921
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
## Abstract The Erbium: Yttrium Aluminum Garnet (YAG) laser used for preparation of cavity can alter the substrate and it could influence the bond strength of enamel. The aim of this __in vitro__ study was to evaluate the influence of Er:YAG laser's energy using microtensile bond test. Three groups
## Abstract ## Background and Objective We have reported that the application of ultrasonic scalers on the Er:YAG laser‐irradiated enamel surface achieved bond strengths of approximately 16 MPa. However, it is reported that a bond strength of 20 MPa is needed to prevent the maginal gaps, so the te
Success in sandwich technique procedures can be achieved through an acceptable bond between the materials. The aim of this study was to compare the effect of 35% phosphoric acid and Er,Cr:YSGG laser on shear bond strength of conventional glass-ionomer cement (GIC) and resin-modified glass-ionomer ce