Microstructure study of laser welding cast nickel-based superalloy K418
โ Scribed by Ming Pang; Gang Yu; Heng-Hai Wang; Cai-Yun Zheng
- Book ID
- 104023205
- Publisher
- Elsevier Science
- Year
- 2008
- Tongue
- English
- Weight
- 1007 KB
- Volume
- 207
- Category
- Article
- ISSN
- 0924-0136
No coin nor oath required. For personal study only.
โฆ Synopsis
Experiments of laser welding cast nickel-based superalloy K418 were conducted. Microstructure of the welded seam was characterized by optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction (XRD), and energy dispersive spectrometer (EDS).
Mechanical properties of the welded seam were evaluated by microhardness. The corresponding mechanisms were discussed in detail. Results show that the laser welded seam have non-equilibrium solidified microstructures consisting of Cr-Ni-Fe-C austenite solid solution dendrites as the dominant and some fine and dispersed Ni 3 (Al,Ti) โฅ phase as well as little amount of MC needle carbides and particles enriched in Nb, Ti and Mo distributed in the interdendritic regions, cracks originated from the liquation of the low melting points eutectics in the HAZ grain boundary are observed, the average microhardness of the welded seam and HAZ is higher than that of the base metal due to alloy elements' redistribution of the strengthening phase โฅ .