𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Microstructure and pitting corrosion of 13CrNiMo weld metals

✍ Scribed by P.D. Bilmes; C.L. Llorente; L. Saire Huamán; L.M. Gassa; C.A. Gervasi


Book ID
116384550
Publisher
Elsevier Science
Year
2006
Tongue
English
Weight
296 KB
Volume
48
Category
Article
ISSN
0010-938X