Microstructure and nanoindentation measurement of residual stress in Fe-based coating by laser cladding
β Scribed by Li-Na Zhu; Bin-Shi Xu; Hai-Dou Wang; Cheng-Biao Wang
- Book ID
- 106397044
- Publisher
- Springer
- Year
- 2011
- Tongue
- English
- Weight
- 649 KB
- Volume
- 47
- Category
- Article
- ISSN
- 0022-2461
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
Fe + 50 wt.% WC composite coating was prepared by laser induction hybrid rapid cladding (LIHRC) on steel substrate. The phase and microstructure of the composite coating were investigated by X-ray diffraction (XRD), environmental scanning electron microscope (ESEM) and energy dispersive spectrum (ED
The in situ synthesized TaC particulate reinforced Ni-based composite coating was fabricated on a mild steel by laser cladding of powder mixture of Ni60 alloy powder with (Ta 2 O 5 + C)-doping. The microstructure and wear resistance of the TaC/Ni60 composite coating were investigated. It is shown th