Microstructure and deformation behavior of Ir-Nb two-phase refractory superalloys for various Nb content

โœ Scribed by Yuefeng Gu; Y Yamabe-Mitarai; Y Ro; H Harada


Book ID
114388783
Publisher
Elsevier Science
Year
1999
Tongue
English
Weight
453 KB
Volume
40
Category
Article
ISSN
1359-6462

No coin nor oath required. For personal study only.