๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Microstructure and creep behavior of A 9%W single crystal nickel-based superalloy

โœ Scribed by Anan Li; Sugui Tian; Fushun Liang; Jingjing Li; Xiaoliang Wang; Te Zhang


Book ID
107669162
Publisher
Nonferrous Metals Society of China
Year
2011
Tongue
English
Weight
505 KB
Volume
30
Category
Article
ISSN
1001-0521

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES