Microfractographic features of crack development in low-temperature low-cycle fatigue of low-nickel steels

โœ Scribed by V. A. Duryagin; I. V. Kokotailo


Publisher
Springer
Year
1982
Tongue
English
Weight
719 KB
Volume
17
Category
Article
ISSN
1573-885X

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Characterization of small crack growth i
โœ J.C. Earthman ๐Ÿ“‚ Article ๐Ÿ“… 1991 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 676 KB

Cylindrical specimens of 12% CrMoV steel were tested under high temperature, low cycle fatigue (HTLCF) conditions to investigate the growth of microcracks which nucleate at the surface. Results are presented which indicate that the microcracks maintain an equilibrium shape under HTLCF conditions, ma