Degradation studies of plasticized PVC.
β
C. A. S. Hill
π
Article
π
1982
π
John Wiley and Sons
π
English
β 713 KB
## Abstract Multiple internal reflection infrared spectroscopy (MIR) was used to study surface degradation in commercial and laboratory prepared plasticized PVC samples. Samples were subjected to accelerated (UV exposure) and natural weathering. Ultravioletβexposed samples show peak formation at 32