Method of accelerated evaluation of Klscc under stress corrosion cracking

✍ Scribed by O.Ye. Andreykiv; M.V. Lysak; V.R. Skalsky


Publisher
Elsevier Science
Year
1996
Tongue
English
Weight
510 KB
Volume
54
Category
Article
ISSN
0013-7944

No coin nor oath required. For personal study only.

✦ Synopsis


The method of accelerated evaluation of the threshold value of stress intensity factor K~,~, in materials under stress corrosion cracking by registration of the crack jumps is proposed. It is based on the model of subcritical jump-like propagation of mode 1 crack as a source of acoustic signals, when material is subjected to the corrosive environment and durable static loading simultaneous effect. The method was experimentally verified during evaluation of K~ of 9HF steel in NaCl water solution and gaseous hydrogen using the up-to-date equipment for recording the acoustic signals.


πŸ“œ SIMILAR VOLUMES


Assessment of test methods for evaluatio
✍ J. Mietz; B. Isecke πŸ“‚ Article πŸ“… 2002 πŸ› John Wiley and Sons 🌐 German βš– 505 KB

Prestressing steels can be exposed in prestressed concrete structures in construction stage (ungrouted duct) to environmental conditions causing formation and growth of hydrogen induced cracks with brittle fracture of the steel. The risk of this hydrogen induced stress corrosion cracking can be mini