๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Mechanochemical model to predict stress corrosion crack growth of stainless steel in high temperature water

โœ Scribed by Koichi Saito; Jiro Kuniya


Book ID
117085641
Publisher
Elsevier Science
Year
2001
Tongue
English
Weight
525 KB
Volume
43
Category
Article
ISSN
0010-938X

No coin nor oath required. For personal study only.