Pyrolyzed, conducting kapton polyimide:
โ
C. Z. Hu; J. D. Andrade
๐
Article
๐
1985
๐
John Wiley and Sons
๐
English
โ 359 KB
Polyimide was pyrolyzed in an argon atmosphere at 900ยฐC for lh. The room temperature conductivity of the polyimide gradually increased from 15 to 100 S/cm with increased pyrolysis time. Further increase in the pyrolysis time did not increase the conductivity. X-ray photcelectron spectroscopy (XPS) s