✦ LIBER ✦
Mechanical behavior under nanoindentation of a new Ni-based glassy alloy produced by melt-spinning and copper mold casting
✍ Scribed by F.S. Santos; J. Sort; J. Fornell; M.D. Baró; S. Suriñach; C. Bolfarini; W.J. Botta; C.S. Kiminami