𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Measurement of the density and surface tension of Ni-based superalloys in the liquid and mushy states

✍ Scribed by Zushu Li; Kenneth C. Mills; Malcolm McLean; Kusuhiro Mukai


Publisher
The Minerals, Metals & Materials Society
Year
2005
Tongue
English
Weight
684 KB
Volume
36
Category
Article
ISSN
1543-1916

No coin nor oath required. For personal study only.