Measurement of Creep Compliance of Solid Polymers by Nanoindentation

โœ Scribed by H. Lu; B. Wang; J. Ma; G. Huang; H. Viswanathan


Book ID
111601216
Publisher
Springer Netherlands
Year
2003
Tongue
English
Weight
233 KB
Volume
7
Category
Article
ISSN
1385-2000

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Measurement of process-dependent materia
โœ Xiangmin Liao; Timothy Scott Wiedmann ๐Ÿ“‚ Article ๐Ÿ“… 2005 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 278 KB

The purpose of this work was to evaluate nanoindentation as a means to characterize the material properties of pharmaceutical solids. X-ray diffraction of potassium chloride and acetaminophen showed that samples prepared by cooling a melt to a crystalline sample as opposed to slow recrystallization