Hot compression tests at different temperatures and strain rates were performed on Inconel 718 solution treated as well as solution treated and then aged at 900ยฐC for 1โ24h in order to investigate the effect of the ฮด phase on hot deformation behavior. A hyperbolic-sine Arrhenius-type equation was us
The hot deformation characteristics of a Ni-base superalloy are studied in the temperature range 1000-1200 ยฐC and strain rate range 0.001-1.0 s ร1 using hot compression tests. Processing maps for hot working are developed on the basis of the variations of efficiency of power dissipation with tempera