Mathematical Model for high temperature properties of cast nickel superalloys with high content of gamma prime phase
✍ Scribed by Dr. sc. techn. A. Efimov
- Publisher
- John Wiley and Sons
- Year
- 1994
- Tongue
- English
- Weight
- 424 KB
- Volume
- 25
- Category
- Article
- ISSN
- 0933-5137
No coin nor oath required. For personal study only.
✦ Synopsis
Abstract
This investigation relates to structural cast superalloys with improved oxidation resistance in the temperature range of 1100–1200°C. It was tried to clarify the role of heavy metal elements on mechanical properties of an alloy in the system Ni‐17at% Al‐3at% Cr‐Mo‐Ta‐W. Solidus temperature, yield strength at 20°C, ultimate tensile strength at 1200°C of polycrystal alloys and creep‐rupture life at 1000°C and 1200°C of single crystals <001> were investigated by means of experimental design and regression analysis techniques, It was determined that solidus temperature do not depend from W content, yield strength at 20°C and ultimate tensile strength at 1200°C strongly depend on Ta and W contents. The properties sharply increase with simultaneous adding of Ta+W. At 1200°C Mo content is a critical factor. The influence of alloying with Ta and W on the creep resistance of single crystals was examined. With increase of test temperature dependence of creep resistance from refractory additives appears to increase, but interval of an optimum alloying narrows.