Magnetomechanical coupling of heat-treated Fe-Si-B metallic glasses
✍ Scribed by Z. Kaczkowski
- Publisher
- Elsevier Science
- Year
- 1990
- Tongue
- English
- Weight
- 269 KB
- Volume
- 161
- Category
- Article
- ISSN
- 0921-4526
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
The specific heats of Fe72NilsZr10, C072.9Cr17.1Zrlo , Ni78Si10B12 and PdsoSi20 amorphous alloys were measured in the temperature range 77-800 K. The magnetic anomaly of the heat capacity at the ferromagnetic Curie temperature T c was observed for Fe-Ni-Zr alloy, but not for Co-Cr-Zr. The results ar
The influence of annealing in vacuum at temperatures of 390 °C for 1/2 h and at 400 °C for 5 min on the magnetomechanical coupling and ultrasound velocities in Fe79SiteB 9 metallic glasses is discussed. Annealing at 390 °C improves the magnetomechanical coupling (kin=0.37). However, after annealing