Magnetic resonance imaging studies on gadonanotube-reinforced biodegradable polymer nanocomposites

✍ Scribed by Balaji Sitharaman; Meike Van Der Zande; Jeyarama S. Ananta; Xinfeng Shi; Andor Veltien; X. Frank Walboomers; Lon J. Wilson; Antonios G. Mikos; Arend Heerschap; John A. Jansen


Book ID
102296841
Publisher
John Wiley and Sons
Year
2009
Tongue
English
Weight
484 KB
Volume
9999A
Category
Article
ISSN
1549-3296

No coin nor oath required. For personal study only.

✦ Synopsis


Abstract

We report about the in vitro cytotoxicity and MRI studies of Gd^3+^ions‐doped ultra‐short single‐walled carbon nanotube (gadonanotubes), gadonanotubes‐ reinforced poly(lactic‐co‐glycolic acid) (PLGA) polymer nanocomposites and in vivo small animal MRI studies using the gadonanotubes. These studies were performed to explore the suitability of gadonanotubes‐reinforced PLGA polymer nanocomposite as a model scaffold for noninvasive magnetic resonance imaging (MRI) to evaluate nanotube release during the degradation process of the scaffold and their biodistribution upon release from the polymer matrix in vivo. The gadonanotubes at 1–100 ppm and the gadonanotubes/PLGA nanocomposites (2 wt % gadonanotubes) did not show any cytotoxicity in vitro as demonstrated using the LIVE/DEAD viability assay. For the first time, r~2~ relaxivity measurements were obtained for the superparamagnetic gadonanotubes. In vitro 7T MRI of the superparamagnetic gadonanotubes ([Gd] = 0.15 m__M__) suspended in a biocompatible 1% Pluronic F127 solution, gave a r~2~ value of 578 m__M__^−1^ s^−1^. Upon subcutaneous injection of the gadonanotubes suspension into the dorsal region of rats, the high r~2~ value translated into excellent and prolonged negative contrast enhancement of in vivo
T~2~weighted proton MRI images. The in vitro characterization of the nanocomposite discs and their degradation process by MRI, showed strong influence of the gadonanotube on water proton relaxations. These results indicate that the gadonanotubes/PLGA nanocomposites are suitable for further in vivo studies to track by MRI the biodegradation release and biodistribution of gadonanotubes. © 2009 Wiley Periodicals, Inc. J Biomed Mater Res, 2010