The effect of a plasma-sprayed hydroxylapatite (HA) coating on the degree of bone ingrowth and interface shear attachment strength was investigated using a canine femoral transcortical implant modeI. Cylindrical implants were fabricated by sintering spherical Co-Cr-Mo particles 500-710 p m in diamet
Long-term ingrowth and apposition of porous hydroxylapatite implants
โ Scribed by Nunes, C. R. ;Simske, S. J. ;Sachdeva, R. ;Wolford, L. M.
- Book ID
- 101256010
- Publisher
- John Wiley and Sons
- Year
- 1997
- Tongue
- English
- Weight
- 198 KB
- Volume
- 36
- Category
- Article
- ISSN
- 0021-9304
No coin nor oath required. For personal study only.
โฆ Synopsis
Bone implant materials are often used to fill in bone gaps that frequently result from orthognathic and craniofacial reconstruction. The substrate hydroxylapatite (HA) is commonly implanted into the bone voids, resulting from these conditions due to its established biocompatibility and osteoconductive properties. The porous structure of HA provides a three-dimensional guideline for fibrovascular ingrowth, facilitating the process that ultimately results in the deposition of new bone. Porous HA (Interpore, 200) implants were implanted in the mandible or maxilla of nine humans and removed after 14-30 months (19.1-month mean). There was no evidence of an inflammatory response. The sample composition and apposition against the implant were determined using point counting and a digitizing tablet and software. Percent ingrowth in available space (%IAS) was defined as %Bone/(%Bone + %Void). A new measure of implant saturation (%IAS-%Apposition of bone) was established to help determine the fundamental manner in which long-term HA implants incorporate bone. In the mean, the samples were composed of 27% bone, 21% void, and 53% implant. The apposition percentages averaged 60% bone, 16% void, and 24% soft tissue. The %IAS averaged 58%, and implant saturation averaged -3%, indicating that a near-balance between the implant and surrounding bone has been established.
๐ SIMILAR VOLUMES
A 5 x 5 x 1-mm uncoated porous nickel-titanium (nitinol) implant was placed 4 mm to either side of the midsection of the frontal bone and 4 mm anterior to the coronal suture of the cranial bone of New Zealand White rabbits. In the other frontal location, a 5 x 5 x 1-mm coralline hydroxyapatite (HA)
The present study addresses two aspects of the use of nitinol in cranial bone defect repair. The first is to verify that there is substantial bone ingrowth into the implant after 6 weeks; the second is to determine the effect of pore size on the ability of bone to grow into the implant during the ea
Tricalcium phosphate (TCP) is an osteoconductive bioceramic which, when applied to a porous-coated prosthesis, may enhance osseous ingrowth and mechanical stability. TCP plasma-sprayed and unsprayed porous-coated tibial intramedullary r o d s were bilaterally implanted in seven adult rabbits. All ra