𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Leachability of degradation products from hard chairside reline resins in artificial saliva: Effect of water-bath post-polymerization treatment

✍ Scribed by Vanessa Migliorini Urban; Ana Lucia Machado; Carlos Eduardo Vergani; Eunice Teresinha Giampaolo; Ana Cláudia Pavarina; Quezia Bezerra Cass


Book ID
101597843
Publisher
John Wiley and Sons
Year
2011
Tongue
English
Weight
306 KB
Volume
123
Category
Article
ISSN
0021-8995

No coin nor oath required. For personal study only.

✦ Synopsis


Abstract

The effect of a post‐polymerization treatment on the leaching of methacrylic acid (MA) and benzoic acid (BA) from the reline resins [Kooliner (K), New Truliner (N), Ufi Gel hard (U), and Tokuso Rebase Fast (T)] was evaluated. Specimens of each material were divided into two groups: Group C (control) – left untreated; Group WB (water‐bath) – immersion in water at 55 ± 1°C for 10 min. Specimens were placed in artificial saliva at 37 ± 1°C and, after 1‐, 3‐, 5‐, 24‐h and 3‐, 7‐, 14‐, and 30‐day intervals, aliquots were removed and analyzed using high performance liquid chromatography. Data were analyzed by using Wilcoxon, Mann–Whitney or Kruskal–Wallis tests (α = 0.05). At 1 h, the concentration of MA released from U control specimens was higher than those of the other ones, and decreased after 3 h. WB specimens released lower amounts of MA than control specimens only for material U, at the 1‐ and 3‐h periods. For all control specimens, concentrations of leached BA progressively decreased within 5 h and from 24 h to the end. WB specimens released significantly lower amounts of BA than did the control groups. The highest concentration of MA was leached from control specimens of Ufi Gel hard. Water‐bath post‐polymerization treatment caused a significant reduction in elution of BA. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011