𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Lattice strain evolution during creep in single-crystal superalloys

✍ Scribed by James Coakley; Roger C. Reed; Jonnathan L.W. Warwick; Khandaker M. Rahman; David Dye


Book ID
113415949
Publisher
Elsevier Science
Year
2012
Tongue
English
Weight
882 KB
Volume
60
Category
Article
ISSN
1359-6454

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Anisotropic strain hardening following l
✍ M.C. Carroll; K. Serin; G. Eggeler πŸ“‚ Article πŸ“… 2004 πŸ› Elsevier Science 🌐 English βš– 402 KB

A critical examination and qualitative evaluation of anisotropic creep behavior in nickel-based superalloy CMSX-4 single crystals is provided with respect to previously established models describing pure shear creep of specimens deformed at high temperatures. Using double-shear creep deformation sam