Investigation of thermal degradation of polystyrene by differential scanning calorimetry
β Scribed by H. K. Toh; B. L. Funt
- Publisher
- John Wiley and Sons
- Year
- 1982
- Tongue
- English
- Weight
- 340 KB
- Volume
- 27
- Category
- Article
- ISSN
- 0021-8995
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
## Abstract Temperature modulated differential scanning calorimetry (TMDSC) was employed to study the melting and crystallization behavior of various polyethylenes (PEs). Samples of high density PE (HDPE), low density PE (LDPE), linear low density PE (LLDPE), and very low density PE (VLDPE) with di
There are many studies on the surface molecular motion of polymer films [1], but no report on surface thermal properties of polymer because of experimental difficulties. The thermal property of oligomeric polystyrene (PS) was investigated by differential scanning calorimetry (DSC) in the present stu