𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Investigation of short fatigue cracks in nickel-based single crystal superalloy SC16 by in-situ SEM fatigue testing

✍ Scribed by X.P Zhang; C.H Wang; W Chen; L Ye; Y.-W Mai


Book ID
114386578
Publisher
Elsevier Science
Year
2001
Tongue
English
Weight
407 KB
Volume
44
Category
Article
ISSN
1359-6462

No coin nor oath required. For personal study only.