Isothermal oxidation of a NiAI/TiB2 composite material has been investigated. Samples of NiAl with 0, l 0 and 20 vol.% TiB 2 particulates were oxidized at 1000, 1100 and 1200Β°C for 48 h. Thermogravimetric analysis was used to quantify oxide growth kinetics. Scanning electron microscopy with energy d
β¦ LIBER β¦
Interfacial behavior in a Ni3Al/TiB2 intermetallic matrix composite
β Scribed by X. Liang; E.J. Lavernia
- Publisher
- Elsevier Science
- Year
- 1992
- Tongue
- English
- Weight
- 941 KB
- Volume
- 153
- Category
- Article
- ISSN
- 0921-5093
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
Oxidation behavior of a NiAl/TiB2 interm
β
B.A Pregger; T Kircher; A Khan
π
Article
π
1992
π
Elsevier Science
π
English
β 848 KB
Interfacial reactions in a Ti-6Al-4V bas
β
M. Ferraris; C. Badini; F. Marino; F. Marchetti; S. Girardi
π
Article
π
1993
π
Springer
π
English
β 709 KB
Corrosion Behavior of Al-based Composite
β
H. Huo; S.βC. Tjong
π
Article
π
2007
π
John Wiley and Sons
π
English
β 672 KB
Friction and wear behavior of Al2O3/TiB2
β
Deng Jianxin; Ai Xing; Li Zhaoqian
π
Article
π
1996
π
Elsevier Science
π
English
β 562 KB
Erratum to βLow-cycle fatigue behavior o
β
S.C. Tjong; G.S. Wang; Y.W. Mai
π
Article
π
2004
π
Elsevier Science
π
English
β 32 KB
Studies on wear behavior of nano-interme
β
D. Roy; S.S. Singh; B. Basu; W. Lojkowski; R. Mitra; I. Manna
π
Article
π
2009
π
Elsevier Science
π
English
β 892 KB
Resistance to wear is an important factor in design and selection of structural components in relative motion against a mating surface. The present work deals with studies on fretting wear behavior of in situ nano-Al 3 Ti reinforced Al-Ti-Si amorphous/nanocrystalline matrix composite, processed by h