The 1150 °C oxidation behavior of γ + γ′-based alloys containing up to 20 at.% Pt and 15-22 at.% Al was investigated in an effort to further develop and optimize alternative bond coating compositions for advanced thermal barrier coating systems. It was found that the co-addition of Pt and Hf was ext
Interdiffusion behavior of Pt-diffused γ + γ′ coatings on Ni-based superalloys
✍ Scribed by Y. Zhang; J.P. Stacy; B.A. Pint; J.A. Haynes; B.T. Hazel; B.A. Nagaraj
- Publisher
- Elsevier Science
- Year
- 2008
- Tongue
- English
- Weight
- 936 KB
- Volume
- 203
- Category
- Article
- ISSN
- 0257-8972
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
Nickel aluminide coatings are used to protect the surfaces of turbine engine hot-stage components. Increasing service temperatures are driving the need for improved performance coatings, which grow and retain thin, protective alumina scales. This paper describes the oxidation resistance of platinum-
The structural and microstructural characterizations of four alloys with nominal compositions of Ti-42Al-2Mo, Ti-42Al-6Mo, Ti-40Al-2Mo, and Ti-40Al-6Mo have been studied. The 2 at.% Mo as cast alloys comprise of (␣ 2 + ␥) phases whereas those of 6 at.% Mo show (B2 + ␥) phases. The solution treatment