𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Initiation and growth of small fatigue cracks in a nickel-base superalloy : Mei, Z., Krenn, C.R. and Morris, J.W. Jr. Metall. Mater. Trans. A (1995) 26A (8), 2063–2073


Book ID
107892065
Publisher
Elsevier Science
Year
1996
Tongue
English
Weight
179 KB
Volume
18
Category
Article
ISSN
0142-1123

No coin nor oath required. For personal study only.