Inhibition effect of metal cations to intergranular stress corrosion cracking of sensitized Type 304 stainless steel

โœ Scribed by Shenghan Zhang; Toshio Shibata; Takumi Haruna


Book ID
116384210
Publisher
Elsevier Science
Year
2005
Tongue
English
Weight
233 KB
Volume
47
Category
Article
ISSN
0010-938X

No coin nor oath required. For personal study only.