Since silica has strong filler-filler interactions and adsorbs polar materials, a silica-filled rubber compound has a poor dispersion of the filler and poor cure characteristics. Improvement of the properties of silica-filled styrene-butadiene rubber (SBR) compounds was studied using acrylonitrile-b
Infrared dichroism and birefringence studies of silica-filled styrene–butadiene rubbers
✍ Scribed by L. Bokobza; L. Ladouce; Y. Bomal; B. Amram
- Publisher
- John Wiley and Sons
- Year
- 2001
- Tongue
- English
- Weight
- 150 KB
- Volume
- 82
- Category
- Article
- ISSN
- 0021-8995
- DOI
- 10.1002/app.1934
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
Bound rubber in a filled rubber compound is formed by physical adsorption and chemisorption between the rubber and the filler. Styrene-butadiene rubber (SBR) is composed of four components of styrene, cis-1,4-, trans-1,4-, and 1,2-units. Fillerpolymer interactions in both silica and carbon black-fil
## Abstract The mechanical properties and morphologies of PP/SBR/SiO~2~ nanocomposites have been studied using mechanical testing, wide‐angle X‐ray diffraction (WAXD), polarizing optical microscopy (POM), scanning electron microscopy (SEM), differential scanning calorimetry (DSC), and thermogravime