Thermoplastic polyurethane elastomers (TPUs) are generally synthesized by using the two-step, so-called prepolymer, method. To study the influence of the prepolymer on the properties of the final TPUs, four polyurethane prepolymers were prepared from a diisocyanate and a macroglycol by using differe
Influence of the synthesis conditions on the properties of thermoplastic polyurethane elastomers
✍ Scribed by M. S. Sánchez–Adsuar; E. Papon; J-J. Villenave
- Publisher
- John Wiley and Sons
- Year
- 2000
- Tongue
- English
- Weight
- 133 KB
- Volume
- 76
- Category
- Article
- ISSN
- 0021-8995
No coin nor oath required. For personal study only.
✦ Synopsis
Thermoplastic polyurethane elastomers (TPUs) of constant composition were prepared by using the prepolymer method and by changing the reaction conditions (prepolymerization and chain-extension time) to study the influence of these conditions on the final TPU properties. The TPUs were characterized by gel permeation chromatography, differential scanning calorimetry, strain-stress measurements, and contactangle measurements. To test the adhesion properties of the TPUs, poly(vinyl chloride) strips were bonded to each other by using TPU solutions and the T-peel strength of the adhesive joints was measured. It was found that provided a threshold is crossed, the prepolymerization time markedly influences the final properties of the TPUs (viscosity of solutions, molecular weight, mechanical and adhesive behavior), whereas the chain extension time does not. Therefore, it is possible to prepare TPUs with specific properties by playing with the prepolymerization conditions.
📜 SIMILAR VOLUMES
The synthesis of thermoplastic polyurethane elastomers (TPUs) is generally carried out using the prepolymer method. To study the influence that the properties of the prepolymer may have in the final TPUs, four TPUs were prepared by using different NCO/OH ratios. The prepolymers and the macroglycol u
Poly(esterurethane) elastomers were synthesized by a pre-polymer process. The pre-polymer based on poly(caprolactone) (capa-225) and toluenediisocyanate (TDI) was mixed with 1,4-butane diol (BDO) or dihydroquinone (HQ) in capa-225 (known as the quasi pre-polymer process) and then reacted in a mould.