𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Influence of hydration on nanoindentation induced energy expenditure of dentin

✍ Scribed by Luiz Eduardo Bertassoni; Michael Vincent Swain


Book ID
116616508
Publisher
Elsevier Science
Year
2012
Tongue
English
Weight
289 KB
Volume
45
Category
Article
ISSN
0021-9290