Influence of coatings on the microstructural degeneration of nickel superalloys
β Scribed by P. Pizzi; S. Tosto; E. Ramous
- Publisher
- Elsevier Science
- Year
- 1979
- Tongue
- English
- Weight
- 58 KB
- Volume
- 64
- Category
- Article
- ISSN
- 0040-6090
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
## Abstract The effect of crystal orientation on the microstructure of a nickelβbased crystalline superalloys during directional solidification was explored. Differently oriented crystals with [001] and [011] orientations were fabricated with seeding technique. The results showed that primary dendr
A diffusion barrier type coating with a duplex layer structure, an inner r-(Re, W, Cr, Ni) as a diffusion barrier and outer Ni-aluminide as an Al reservoir, was formed on a Nickel based, single crystal, superalloy (TMS-82 +) and on Hastelloy X. Oxidation properties of both the alloys with or without