Inertia Friction Welding Dissimilar Nickel-Based Superalloys Alloy 720Li to IN718

โœ Scribed by Z.W. Huang; H.Y. Li; M. Preuss; M. Karadge; P. Bowen; S. Bray; G. Baxter


Book ID
107441408
Publisher
The Minerals, Metals & Materials Society
Year
2007
Tongue
English
Weight
828 KB
Volume
38
Category
Article