π SIMILAR VOLUMES
Depth-sensing indentation measurements were performed using the three trihedral pyramid indenters with the specific inclined face angles Ξ² B (Ξ² B = 11.4 β’ , 24.7 β’ (Berkovich) and 43.7 β’ ), three tetrahedral pyramid indenters with Ξ² V (Ξ² V = 10 β’ , 22 β’ (Vickers) and 40 β’ ) and a Knoop indenter (Ξ² K
## Abstract The fracture behavior and deformation mechanism of polypropylene (PP)/ethyleneβoctene copolymer (POE)/magnesium hydroxide [Mg(OH)~2~] ternary composites were investigated. The fracture behavior of the PP/POE/Mg(OH)~2~ ternary composites was strongly influenced by the POE content. In the