Nanograined (grain size 10 nm) ZnO films with various Co contents (0-52 at.% Co) were synthesized by a novel liquid ceramics method. The solubility limit for Co was determined at 550 Β°C. The lattice parameter c of the ZnO-based solid solution with wu Β¨rzite structure ceases to grow at 33 at.% Co. The peaks of the second phase (Co 2 O 3 or with cubic lattice) become visible in the X-ray diffraction spectra at 40 at.% Co. The same second phase appears in the bulk ZnO already at 2 at.% Co [Bates CH, White WB, Roy R. J Inorg Nucl Chem 1966;28:397]. A few years ago it was predicted theoretically that ZnO could become ferromagnetic at room temperature and above by doping with Co and other transition metals. Recently published papers on the structure and magnetic behaviour of Co-doped ZnO allowed us to obtain the size dependence of Co solubility in ZnO for the polycrystals and small single-crystalline particles. The overall Co solubility drastically increases with decreasing grain size. The quantitative estimation leads to the conclusion that, close to the bulk solubility limit, the thickness of a Co-enriched layer is several monolayers in grain boundaries and at least two monolayers in the free surfaces.


πŸ“œ SIMILAR VOLUMES


Increase of Mn solubility with decreasin
✍ Boris Straumal; Brigitte Baretzky; Andrei Mazilkin; Svetlana Protasova; Ata Myat πŸ“‚ Article πŸ“… 2009 πŸ› Elsevier Science 🌐 English βš– 340 KB

Nanograined (grain size 20 nm) ZnO films with various Mn content (from 0 to 47 at%) were synthesized by the novel wet chemistry method. The solubility limit for Mn was determined at 550 β€’ C. The lattice parameter c of the ZnO-based solid solution with wurzite structure ceases to grow at 30 at% Mn. T