In situ synchrotron X-ray micro-tomography study of pitting corrosion in stainless steel

✍ Scribed by S. Majid Ghahari; Alison J. Davenport; Trevor Rayment; Thomas Suter; Jean-Philippe Tinnes; Cristiano Padovani; Joshua A. Hammons; Marco Stampanoni; Federica Marone; Rajmund Mokso


Book ID
116385739
Publisher
Elsevier Science
Year
2011
Tongue
English
Weight
549 KB
Volume
53
Category
Article
ISSN
0010-938X