𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Improved Resistance to Stress-Corrosion-Cracking FailuresviaOptimized Retrogression and Reaging of 7075-T6 Aluminum Sheets

✍ Scribed by Murat Baydogan; Huseyin Cimenoglu; E. Sabri Kayali; Jahan Rasty


Book ID
107443605
Publisher
The Minerals, Metals & Materials Society
Year
2008
Tongue
English
Weight
512 KB
Volume
39
Category
Article
ISSN
1073-5623

No coin nor oath required. For personal study only.