Simulation of hydrogen assisted stress c
✍
I. Scheider; M. Pfuff; W. Dietzel
📂
Article
📅
2008
🏛
Elsevier Science
🌐
English
⚖ 241 KB
This paper investigates the effect of hydrogen diffusion on stable crack propagation by using numerical finite element simulations based on the cohesive model. The model with its two common parameters, cohesive strength, T 0 , and critical separation, d 0 , and its two additional parameters for stre