High-temperature strength of nickel-bsed superalloys for the construction of gas turbines from a metallographic point of view [hochwarmfestigkeit von nickelbasis-superlegierungen für den gasturbinenbau aus metallkund-licher sicht]: Heine, N. Metall (1995) 49 (6), 393–398, 400