Tensile behavior of a cast Ni-base superalloy M963 under solution treatment and age treatment was studied in the temperature range from 20 to 1100 β’ C. Extensive TEM investigations were performed after tensile test to fracture. Furthermore, the fracture surfaces were studied in the SEM. The yield an
Nickel-based superalloy single crystal specimens have been tested under anisothermal creep conditions using two different routes, both including an overheating stage. In the first route, the material is tested under creep conditions at 1050 β’ C, then submitted to an overheating regime at 1200 β’ C, a